After much messin around, I'm finally starting to get somewhere with this.

The pic is the coupon after another 3 rusts, (2 two hr rusts and one 11 hr rust) and boiling after each, then finally after the 3 consecutive rusts/boil/carding, one 5 second etch in a solution of 1.5 oz Radio Shack etch/8.5 oz water. I played with the lightness/darkness of the pic to make it look like actual, but did not adjust contrast. Oh, and I went courser on the steelwool to "0" grade

Last edited by Chuck H; 01/11/08 09:50 PM.