I have a couple of British side by sides that have been sleeved. Both have problems with fired shells sticking in the chambers. I've tried "polishing" the chambers with abrasive cloth on a dowel and that polishing does seem to help a little bit, but does not totally eliminate the problem. The forcing cones of both guns appear to be very rough but I don't have a bore scope to get a real good look at that area. I see that Flex Hone has both chamber hones and forcing cone hones in several grits. I'm wondering if anyone has experience with the hones and could recommend what grit to use and any special tecnique?
Gary Erickson