Joined: Jan 2002
Posts: 11,139 Likes: 1654
Sidelock
|
Sidelock
Joined: Jan 2002
Posts: 11,139 Likes: 1654 |
Can you post a photo of the name, on the opening lever? Id love to see a clear shot of the proof marks on the barrel flats, as well, if you could.
Thanks in advance, Ted
|
|
|
|
|
Joined: Jun 2002
Posts: 2,354 Likes: 107
Sidelock
|
OP
Sidelock
Joined: Jun 2002
Posts: 2,354 Likes: 107 |
No name on the lever. But stamped Darne on top of breech. 
|
|
|
|
|
Joined: Dec 2001
Posts: 2,961 Likes: 9
Sidelock
|
Sidelock
Joined: Dec 2001
Posts: 2,961 Likes: 9 |
Just repaired a SLE splinter forend where the junction of the wood and forend iron were about .015 different. I made a batch of garnet shelllac and applied several coats until the finish height and metal were the same height. It took about 6 days of coating, sanding , slectively coating. Before it was right. The garnet shellac finish matched this medimum grade British gun. Be ready to spend a lot of time!
bill
|
|
|
|
|
Joined: Jun 2002
Posts: 2,354 Likes: 107
Sidelock
|
OP
Sidelock
Joined: Jun 2002
Posts: 2,354 Likes: 107 |
Just repaired a SLE splinter forend where the junction of the wood and forend iron were about .015 different. I made a batch of garnet shelllac and applied several coats until the finish height and metal were the same height. It took about 6 days of coating, sanding , slectively coating. Before it was right. The garnet shellac finish matched this medimum grade British gun. Be ready to spend a lot of time!
bill Did it match the rest of the refinish? Can you show a pic?
|
|
|
|
|
|
|