Fibre wads (dry) in plastic hulls, usually Federal Top Gun, once and done.
80 grains FFg, 1 1/8 ounce #8 shot.
I don't use shot cups because they didn't improve patterns over no shot cup, in fact worse.
I have been using a dab of lube on the crimp for at least 25 years. It sure eases cleaning.
There is no lube migration on hot days if you don't use lubed wads in your load.
We use a cartridge block to hold and carry our shells crimp up.