Soft solder usually flows around 400-450 degrees. If a rib seperates from the barrels during use its not because of heat.
The blame would probably be more along the lines of a poor bond between solder and metal, or the rib not being fit/smoked tight on the barrels.

Last edited by gunmaker; 09/04/13 07:47 PM.