At least with plastic shells, you seem to get some "nose-coning" after you've used the same hull several times. I can notice a definite difference between once or twice fired hulls and 8 or 10 times fired hulls. And that's in 2 3/4" chambers.

I doubt I'd have cones done for the relatively little pressure reduction either, but it was an interesting result of Bell's tests.