For lead/tin soldering, I've never had any success tinning bare steel with rosin flux. I tin the components to be soldered with acid based flux, scrub them thoroughly with a scouring pad and soap, then solder the tinned parts with rosin based flux. Same for using Brownells HiForce 44.

Last edited by Chuck H; 07/29/19 08:12 AM.