Feeling great about success today about gettting my Field SLE project back on face by TIG welding, smoking, and filing. I've failed at that task before, so I guess I learned from it.

The weld cooled slowly, and I'm wondering if it needs to be hardened. If so, how do you heat it but not compromise the solder, etc.? If not, thanks for reading the post nonetheless.