Originally Posted By: Stan
From another thread I posted on:

All is not lost. You can get low pressures with other powders, too. The last loads I had Tom Armbrust test was with Solo 1000.

Average for five:

1192 fps
5182 psi
1 oz. 7 1/2s

These were in either STS or Nitro hulls, not AAs, but I really wouldn't expect much difference as they are all compression formed hulls. Might want to send a sample to Tom to make sure, tho'.

SRH

On second thought, I need to check and make certain which hull I loaded those in. The letter from Tom A. is out in the shop. I'll get back to you on it, to be certain. Don't want to post any misinformation.

SRH


It was STS hulls, the wad was Claybuster 1100-12, and the primers were Cheddite 209, charge was 18.1 grs. Solo 1000.

SRH